PRIMER EPOXY A+B
priming
For the current use, mix 1 kg of soil (A) with 0.11 kg of catalyst (B). The product prepared in this way should be applied to the substrate, thoroughly rubbed in with a thin layer. Priming strengthens and prevents excessive absorption, bonding the substrate increases the adhesion and performance of subsequent layers. Use prepared material within 1 hour.

OXIDECOR EPOXY
decorative coat
Mix component A (resin) with component B (catalytic agent) and stir thoroughly. Apply the first layer of Oxidecor Epoxy and distribute an appropriate amount evenly using a metal trowel (1kg / 1m2). Produce a regular texture on a fresh coat using a knit roller, moving it in multiple directions. Apply Aktywator New to a coat of Oxidecor Epoxy using an atomiser. The work should be performed in stages, applying the compound to small areas until the whole surface is covered. Use prepared material within 1 hour.

AKTYWATOR NEW WARSTWA AKTYWUJĄCA
activating layer
Apply Aktywator New to a coat of Oxidecor Epoxy using an atomiser. Keep in mind that the amount of using the atomiser depends on the drying time of the coat, the slower it dries, the more discolouration will be produced. This results from various factors such as humidity, temperature, and draughts. Do not perform work in the sun, rain, wind, and at temperatures below 0°C. Leave to dry.

A18
base coat

EPOXON TRANSPARENT GLOSS
protective layer
Epoxon Transparent Gloss must be mixed with hardening agent (100:26). Mix component A (resin) with component B (catalytic agent), stir thoroughly. Apply to the substrate using a roller until the whole substrate is covered. Ready to use up to 1 h after mixing. Although its look and consistency may seem to be right, do not use after this period as it will not present proper characteristics!!!

EPOXON TRANSPARENT GLOSS LUB SATIN
protective layer
Epoxon Transparent must be mixed with hardening agent (100:26). Mix component A (resin) with component B (catalytic agent), stir thoroughly. Apply to the substrate using a roller until the whole substrate is covered. Ready to use up to 1 h after mixing. Although its look and consistency may seem to be right, do not use after this period as it will not present proper characteristics!!!